Chrome Plated is a galvanizing, based on electrolysis , by means of which a thin layer of metallic chrome is deposited on metallic objects and even on plastic material. Electrolytic chrome plating is extensively used in industry to protect metals from corrosion, improve appearance and performance.
Summary
[ hide ]
- 1 hard chrome
- 2 External and internal chrome
- 1 Chrome for plastic surfaces
- 2 Electrolytic Solution
- 3 Anodic and Cathodic Reactions
- 4 Temperature
- 3 Performance and intensity
- 4 Chrome Paint
- 1 How they work
- 5 external links
- 6 sources
hard chrome
The so-called hard chrome are relatively thick electrolytic deposits (0.1 mm) that are deposited on parts that must withstand high wear stresses. This type of deposits are made especially in valve seats, crankshaft bearings, hydraulic piston shafts and in general in places where enough hardness and precision are required.
Bright or decorative chrome are thin layers of chrome that are deposited on copper, brass or nickel to improve the appearance of some objects. The domestic faucet is an example of chrome pieces to give embellishment.
Chromium has little protective power, even less if the layers that are deposited are as thin as one micron. For this reason, the surfaces to be covered must be well polished, shiny and degreased. Chromium works well on copper, nickel, and steel, but not on zinc or cast iron.
External and internal chrome
In a chrome electrolytic bath, chromic acid is dissolved in water at a rate of 300 grams per liter and 2 grams per liter of sulfuric acid is added. A lead or graphite electrode is used as the anode. Lead serves as an anode because a lead oxide plate is formed that is conductive but prevents further corrosion by anodic oxidation. Unlike in other baths such as those for nickel, the chromium that is deposited on the cathode comes from dissolved chromic acid and not from the anode, so the solution gradually becomes poorer in chromium. Chromium depletes with use and must be replenished by adding more chromic acid.
Chrome for plastic surfaces
Hexavalent chromium (Cr(VI)) is the material most used by most companies dedicated to metal plating, specifically chrome plating. One of the great disadvantages of this material is its carcinogenic potential. A new process is being developed based on molecular self-assembly technology (SAM – self assembly methodology) through the use of nano-particles, which will make it possible to avoid the use of this material. This technique has already been developed on a laboratory scale in Spain.
The main objectives of the project are:
- Develop an integrated chrome plating process for plastic surfaces. Said process will be low cost and environmentally sustainable, eliminating the use of: chromic acid, palladium catalysts and nickel electrochemical deposits.
- Reduce the time and number of tanks (chroming and rinsing) necessary in the process (this implies a reduction in water consumption and waste).
- Offer flexibility in the type of plastic materials to be used. The new chrome system can be applied to ABS, PP, PET and PVC.
- Increase the stability of the process compared to the classic chemicalmetallization process .
Electrolyte Solution
Chromic acid is a strong acid and is supplied for chrome plating as dark red flakes; it must be absolutely free of excess sulfuric acid or sulfate because of the dangerous effect of the concentration of these acid catalysts on the way the solution works. Necessary is constant agitation to guarantee homogenization of temperature and solutions.
Anodic and Cathodic Reactions
In the course of electrolysis, part of the hexavalent chromium content of the solution is reduced at the cathode to the trivalent form; Although some degree of oxidation does take place at the anode, it is by no means complete, so trivalent chromium compounds, ie, chromium sulfate, and chromic dichromate, accumulate in solution during normal operation. Although some is lost by “carryover”, its concentration should not be allowed to become excessive, since trivalent chromium compounds have the effect of narrowing the limits of the working conditions of the bright chrome plating solution and lowering its conductivity. . On the other hand, a moderate concentration of trivalent chromium seems to increase somewhat the penetrating power of the solution. If it is necessary to reduce the sulfate content,
Temperature
Due to the extreme hardness of chrome deposits and the natural difficulty of polishing them, it is best, if possible, to produce bright coatings directly from solution. In general, the limits of the bright coating conditions are a function of temperature and current intensity; higher temperatures are needed the higher the current intensity. Bright deposits cannot easily be obtained at temperatures below about 27°C or at current intensities less than 4.3 amps per dm2. Solution temperature control within a narrow range is necessary due to the marked influence of temperature on deposition rate and deposit quality. A 2°C rise in solution temperature means, for example, can cause a reduction of 5% or more in average chrome thickness, requiring considerable adjustment in either plating time or current density. The temperature of the solution must be maintained, it is usually controlled automatically. Manual control is impractical for a production operation.
Performance and intensity
The cathodic efficiency or performance of a chrome plating solution, even under the best conditions, is very low. It is higher when the bath works cold, and yields of 35 to 40% can then be obtained. However, the deposits obtained under these conditions are caramelized and hard. Within the limits of the glossy coating, that is, at temperatures of about 38 to 43°C, the yield is much lower and does not usually exceed 10 to 15%. In practice, current intensities of 11 to 21 amps per dm2 are most commonly used; the voltages usually needed are 5 to 8 volts with low density solutions, or 4 to 6 volts with higher density, more conductive solutions. For the electrolysis of chromium it is convenient to use filtered direct current. It is not convenient to use unfiltered half-wave rectified current since at times when the voltage is zero, the chromic acid attacks the chromium, passivating it. When passivated, the electrical resistance of the chromium increases and the adherence of the subsequent layers decreases. In the same way, the pieces to be chromed should not be left immersed in the electrolyte without current and when they are immersed for the first time they must have the current connected.
Chrome Paint
Splendor Chrome Paint is a long-lasting paint applied in a 3-layer system in a specific order that adheres to all types of materials. The use of conventional systems for chrome plating or any other method of plating metals on surfaces is limited and expensive. The Splendor Chrome Paint application system is being used in various applications to efficiently give a metallic finish with a chrome effect to various materials in different industries.
How do they work
. Base Layer. Applied depending on the surface of the object, this is an automotive grade clear coat.
.Splendor chrome paint.
This 8 step process creates the metallic chrome or mirror effect layer on the object. The specific steps are: 1. Deionized Water, 2. Reducer, 3. Deionized Water, 4. Splendor Chrome Coat, 5. Deionized Water, 6. Antioxidant, 7. Deionized Water, and 8 Drying with pressurized air.
. Protective layer. This is the same material as the base layer. Automotive grade, tintable, clear topcoat. As required, the finish can vary from glossy to matte mirror.